Application:
Stoneware body with cellulose fibre which makes the body less drying sensitive.
Application temperature: 1000 - 1280°C
Specifications:
Grog / Graining:Faser
Drying shrinkage: 5.7 %
1050°C: 1.6% Firing shrinkage / 14.0% Water absorption
1160°C: 5.0% Firing shrinkage / 7.0% Water absorption
1260°C: 6.2% Firing shrinkage / 2.0% Water absorption
Sintering (WA ≤2%) 1260°C.
TEC (20-400°C) 56 * 10-7/K (Pre-firing: 1200°C)